MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Iron (II, III) Oxide, Fe3O4 (Magnetite)
Categories: Ceramic; Oxide

Material Notes: Black cubic crystals or amorphous powder. Weathering end product(s): Limonite, ochre. Occurrence: Igneous rocks, metamorphic. Weathers very slowly to limonite.

Property values are typical of naturally occurring Magnetite (Fe3O4). Actual property values will vary from sample to sample.

Key Words: Fe3O4, Iron Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.17 g/cc0.187 lb/in³
a Lattice Constant 8.394 Å8.394 Å
Formula Units/Cell (Z) 88
Molecular Weight 231.533 g/mol231.533 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 5.55.5
 6.06.0
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 596 J/g256 BTU/lb
CTE, linear  9.20 µm/m-°C
@Temperature 20.0 - 200 °C
5.11 µin/in-°F
@Temperature 68.0 - 392 °F
calculated from volumetric expansion
 13.1 µm/m-°C
@Temperature 20.0 - 500 °C
7.28 µin/in-°F
@Temperature 68.0 - 932 °F
calculated from volumetric expansion
Melting Point 1597 °C2907 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 2.42
@Wavelength 589.3 nm
2.42
@Wavelength 589.3 nm
η, Na
 
Descriptive Properties
CAS Number1317-61-9
ColorBlack
Crystal StructureCubicSpinel

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iron (III) Oxide, Fe2O3 (Hematite)
Iron (III) Oxide, Fe2O3 (Maghemite)
Iron, Fe
Copper, Cu; Annealed
Overview of materials for Low Alloy Steel

EINOR0366 / 3495

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.