MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Refractory Composites RSMAT-3000 ALUMINA MAT
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot and has a higher alumina content than any other ceramic fiber mat or blanket. Type RSMAT-3000 is lightweight, has low thermal conductivity and low heat capacity, and is immune to thermal shock. It is ideal for vacuum, reducing atmospheres and other applications where silica cannot be tolerated, such as powder metal sintering, stainless steel bright annealing and many fuel cell applications.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.0350 g/cc0.00126 lb/in³
Loss On Ignition 0.00 %
@Temperature 800 °C,
Time 7200 sec
0.00 %
@Temperature 1470 °F,
Time 2.00 hour
Filament Diameter 3.0 - 5.0 µm3.0 - 5.0 µm
Thickness 35000 microns1378 mil
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) 875 ppm875 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.06.0
Tensile Strength, Ultimate 0.0350 MPa5.08 psi
Modulus of Elasticity 320 GPa46400 ksi
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.047 J/g-°C0.2502 BTU/lb-°F
Thermal Conductivity  0.0700 W/m-K
@Temperature 315 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 599 °F
parallel to thickness; ASTM C177
 0.130 W/m-K
@Temperature 760 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 1400 °F
parallel to thickness; ASTM C177
 0.300 W/m-K
@Temperature 1425 °C
2.08 BTU-in/hr-ft²-°F
@Temperature 2597 °F
parallel to thickness; ASTM C177
Melting Point 2036 °C3697 °F
Maximum Service Temperature, Air 1650 °C3000 °F
Shrinkage  2.2 %
@Temperature 1425 °C,
Time 86400 sec
2.2 %
@Temperature 2597 °F,
Time 24.0 hour
Linear Reheat Shrinkage
 3.0 %
@Temperature 1535 °C,
Time 86400 sec
3.0 %
@Temperature 2795 °F,
Time 24.0 hour
Linear Reheat Shrinkage
 4.0 %
@Temperature 1650 °C,
Time 86400 sec
4.0 %
@Temperature 3000 °F,
Time 24.0 hour
Linear Reheat Shrinkage
 
Component Elements PropertiesMetricEnglishComments
Al2O3 97 %97 %
Other <= 0.50 %<= 0.50 %
SiO2 3.0 %3.0 %
 
Descriptive Properties
Calcium, ppm525
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-99-45 Refractory Sheet
Zircar Refractory Composites RS-A3 Refractory Sheet
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
Zircar Refractory Composites RS-99-60 Refractory Sheet
DWA 6092/SiC/40p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)

CZRCI44 / 2907

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.