MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DWA 6092/SiC/40p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: A powder metallurgy highly loaded Al MMC comprised of AA6092 aluminum and 40 Vol% Silicon Carbide particles; available in vacuum-hot-pressed billet, extruded, and forged product forms. AA6092 for maximized strength in the billet form. Minimum Coefficient-of-Thermal-Expansion (CTE) and maximum elastic modulus are the material property objectives of highly loaded Al MMCs.

Information provided by DWA Aluminum Composites.

Key Words: AlSiC MMC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.92 g/cc0.105 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 86 - 8886 - 88
Tensile Strength, Ultimate 565 MPa81900 psiExtruded - L and LT orientations
Tensile Strength, Yield 517 MPa75000 psiExtruded - L and LT orientations
Elongation at Break 1.5 %1.5 %Extruded - L and LT orientations
Modulus of Elasticity 138 GPa20000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.1 µm/m-°C6.72 µin/in-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 95.6 - 98 %95.6 - 98 %As Balance, Metal Alloy Basis
Copper, Cu 0.70 - 1.0 %0.70 - 1.0 %Metal Alloy Basis
Iron, Fe <= 0.30 %<= 0.30 %Metal Alloy Basis
Magnesium, Mg 0.80 - 1.2 %0.80 - 1.2 %Metal Alloy Basis
Other, each <= 0.050 %<= 0.050 %Metal Alloy Basis
Other, total <= 0.15 %<= 0.15 %Metal Alloy Basis
Oxygen, O 0.050 - 0.50 %0.050 - 0.50 %Metal Alloy Basis
Silicon, Si 0.40 - 0.80 %0.40 - 0.80 %Metal Alloy Basis
Titanium, Ti <= 0.15 %<= 0.15 %Metal Alloy Basis
Zinc, Zn <= 0.25 %<= 0.25 %Metal Alloy Basis

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DWA 6092/SiC/17.5p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Sheet
DWA 6092/SiC/25p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Extruded
DWA 6092/SiC/17.5p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Extruded
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
DWA 6091/SiC/40p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)

NDWA83 / 231156

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.