MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Kennametal Stellite Stellite® 6 PM cast
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Adhesive wear test data: 0.49 P/M, 0.48 Cast; Typical applications include: (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Data provide by the manufacturer, Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.20 g/cc0.296 lb/in³P/M (98%)
 8.38 g/cc0.303 lb/in³theoretical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 364364Converted from Rockwell C hardness.
 224
@Temperature 760 °C
224
@Temperature 1400 °F
Converted from Rockwell C hardness
 312
@Temperature 649 °C
312
@Temperature 1200 °F
Converted from Rockwell C hardness
 345
@Temperature 538 °C
345
@Temperature 1000 °F
Converted from Rockwell C hardness
Hardness, Knoop 436436Converted from Rockwell C hardness.
 262
@Temperature 760 °C
262
@Temperature 1400 °F
Converted from Rockwell C hardness
 372
@Temperature 649 °C
372
@Temperature 1200 °F
Converted from Rockwell C hardness
 413
@Temperature 538 °C
413
@Temperature 1000 °F
Converted from Rockwell C hardness
Hardness, Rockwell A 7070Converted from Rockwell C hardness.
 60
@Temperature 760 °C
60
@Temperature 1400 °F
Converted from Rockwell C hardness
 67
@Temperature 649 °C
67
@Temperature 1200 °F
Converted from Rockwell C hardness
 69
@Temperature 538 °C
69
@Temperature 1000 °F
Converted from Rockwell C hardness
Hardness, Rockwell C 4040
 19
@Temperature 760 °C
19
@Temperature 1400 °F
 34
@Temperature 649 °C
34
@Temperature 1200 °F
 38
@Temperature 538 °C
38
@Temperature 1000 °F
Hardness, Vickers 383383Converted from Rockwell C hardness.
 230
@Temperature 760 °C
230
@Temperature 1400 °F
Converted from Rockwell C hardness
 326
@Temperature 649 °C
326
@Temperature 1200 °F
Converted from Rockwell C hardness
 362
@Temperature 538 °C
362
@Temperature 1000 °F
Converted from Rockwell C hardness
Tensile Strength, Ultimate 911 MPa132000 psi
 552 MPa
@Temperature 760 °C
80100 psi
@Temperature 1400 °F
 676 MPa
@Temperature 649 °C
98000 psi
@Temperature 1200 °F
 759 MPa
@Temperature 538 °C
110000 psi
@Temperature 1000 °F
Elongation at Break <= 1.0 %<= 1.0 %in 25.4 mm
 1.0 %
@Temperature 538 °C
1.0 %
@Temperature 1000 °F
in 25.4 mm
 2.0 %
@Temperature 649 °C
2.0 %
@Temperature 1200 °F
in 25.4 mm
 5.0 %
@Temperature 760 °C
5.0 %
@Temperature 1400 °F
in 25.4 mm
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability <= 1.2
@Temperature 22.0 °C
<= 1.2
@Temperature 71.6 °F
200 Oersted
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.9 µm/m-°C
@Temperature 0.000 - 100 °C
7.72 µin/in-°F
@Temperature 32.0 - 212 °F
 14.1 µm/m-°C
@Temperature 0.000 - 200 °C
7.83 µin/in-°F
@Temperature 32.0 - 392 °F
 14.5 µm/m-°C
@Temperature 0.000 - 300 °C
8.06 µin/in-°F
@Temperature 32.0 - 572 °F
 14.7 µm/m-°C
@Temperature 0.000 - 400 °C
8.17 µin/in-°F
@Temperature 32.0 - 752 °F
 15.0 µm/m-°C
@Temperature 0.000 - 500 °C
8.33 µin/in-°F
@Temperature 32.0 - 932 °F
 15.3 µm/m-°C
@Temperature 0.000 - 600 °C
8.50 µin/in-°F
@Temperature 32.0 - 1110 °F
 15.8 µm/m-°C
@Temperature 0.000 - 700 °C
8.78 µin/in-°F
@Temperature 32.0 - 1290 °F
 16.3 µm/m-°C
@Temperature 0.000 - 800 °C
9.06 µin/in-°F
@Temperature 32.0 - 1470 °F
 16.9 µm/m-°C
@Temperature 0.000 - 900 °C
9.39 µin/in-°F
@Temperature 32.0 - 1650 °F
 17.4 µm/m-°C
@Temperature 0.000 - 1000 °C
9.67 µin/in-°F
@Temperature 32.0 - 1830 °F
Melting Point 1260 - 1357 °C2300 - 2475 °F
Solidus 1260 °C2300 °F
Liquidus 1357 °C2475 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B <= 1.0 %<= 1.0 %
Carbon, C 1.2 %1.2 %
Chromium, Cr 29 %29 %
Cobalt, Co 52.3 %52.3 %As remainder
Iron, Fe <= 3.0 %<= 3.0 %
Manganese, Mn 1.0 %1.0 %
Molybdenum, Mo <= 1.5 %<= 1.5 %
Nickel, Ni <= 3.0 %<= 3.0 %
Other <= 2.0 %<= 2.0 %
Silicon, Si <= 1.5 %<= 1.5 %
Tungsten, W 4.5 %4.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 6 PM with P/M Processing
Kennametal Stellite Stoody® 6 Cobalt-Base Cast Alloy
Kennametal Stellite Stellite® 3 PM with P/M Processing
Kennametal Stellite Stellite® 12
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy

NS6PMB / 18881

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.