MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials NX10 Boron Nitride (BN) Powder  (discontinued **)
Categories: Ceramic; Nitride; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.

NX grades are all fine hexagonal crystalline powders (95%-100% -325 mesh), and are available in a range of purities and surface areas to suit specific applications.

NX10 has a mean particle size of approximately 10 microns and is a higher purity grade than NX9.

Applications: GE Advanced Ceramics NX grades are candidates for use in a wide range of demanding applications for which BN is generally considered, including:

  • Lubricants and release agents for high-temperature metal & glass processing
  • Refractory coatings
  • Base material for hot pressed solids and metal-matrix or ceramic-metal composites
  • Processing and final-product enhancement of plastics, including nucleation of solid and foamed products.
  • Thermal management materials (adhesives, gap-fillers, encapsulants, polymer matrices, etc.) for electronics applications

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 g/ccTap Density
Particle Size 0.20 - 0.50 µmCrystal Size
 10 µmMean
Specific Surface Area 14 m²/g
 
Descriptive Properties
CalciumMax 0.01 %
Carbon0.1%
ColorWhite
Crystal TypeHexagonal (Graphitic)
Oxygen0.9-1.2%
Sol. Borate0.1%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tellurium, Te
Titanium Nitride (TiN) Coating
MarkeTech Gallium Phosphide Semiconductor Wafer, n-type, Sulfur + Tellurium Doped, Czochralski-LEC Grown
MarkeTech Gallium Arsenide Semiconductor Wafer, Semi-Insulating Undoped, LEC Grown
MarkeTech Gallium Arsenide Semiconductor Wafer, Semi-Insulating Chromium Doped, LEC Grown

CADV27 / 419

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.