MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tellurium, Te
Categories: Metal; Nonferrous Metal; Other Engineering Material; Semiconductor; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.23 g/cc0.225 lb/in³
a Lattice Constant 4.45 Å4.45 Å
c Lattice Constant 5.91 Å5.91 Å
Vapor Pressure  0.001013 bar
@Temperature 505 °C
0.7598 torr
@Temperature 941 °F
 0.01013 bar
@Temperature 617 °C
7.598 torr
@Temperature 1140 °F
 0.1013 bar
@Temperature 768 °C
75.98 torr
@Temperature 1410 °F
 1.013 bar
@Temperature 988 °C
759.8 torr
@Temperature 1810 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 127.60127.601995
Atomic Number 5252
Thermal Neutron Cross Section 4.7 barns/atom4.7 barns/atom
X-ray Absorption Edge 0.38972 Å0.38972 ÅK
 2.50272 Å2.50272 ÅLI
 2.68253 Å2.68253 ÅLII
 2.85162 Å2.85162 ÅLIII
Electronegativity 2.12.1Pauling
Ionic Radius 0.560 Å0.560 ÅCrystal Ionic Radius for Valence +6
 0.700 Å0.700 ÅCrystal Ionic Radius for Valence +4
 0.820 Å0.820 ÅCrystal Ionic Radius for Valence +1
 2.11 Å2.11 ÅCrystal Ionic Radius for Valence -2
 2.50 Å2.50 ÅCrystal Ionic Radius for Valence -1
Electrochemical Equivalent 0.99 g/A/h0.99 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 2525
Tensile Strength, Ultimate 11.0 MPa1600 psi
Modulus of Elasticity 40.0 GPa5800 ksi
Poissons Ratio 0.330.33
Shear Modulus 15.16 GPa2199 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000150 ohm-cm0.000150 ohm-cm
Magnetic Susceptibility -0.0000395-0.0000395Atomic (cgs)
 -3.10e-7-3.10e-7cgs/g
Critical Superconducting Temperature  2.40 - 5.10 K
@Pressure 3800 - 5500 MPa
2.40 - 5.10 K
@Pressure 551000 - 798000 psi
Te II
 4.10 - 4.50 K
@Pressure 5300 - 6200 MPa
4.10 - 4.50 K
@Pressure 769000 - 899000 psi
Te III
 >= 4.72 K
@Pressure 6300 - 8000 MPa
>= 4.72 K
@Pressure 914000 - 1.16e+6 psi
Te IV
Band Gap 0.33 eV0.33 eV
Electron Mobility, cm²/V-s 17001700
Hole Mobility, cm²/V-s 12001200
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 30.6 J/g13.2 BTU/lb
Heat of Vaporization 666 J/g287 BTU/lb
CTE, linear 16.8 µm/m-°C
@Temperature 20.0 - 100 °C
9.33 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.1965 J/g-°C0.04696 BTU/lb-°F
Thermal Conductivity 1.97 W/m-K13.7 BTU-in/hr-ft²-°FPerpendicular to c-axis
 3.38 W/m-K23.5 BTU-in/hr-ft²-°FParallel to c-axis
Melting Point 449.5 °C841.1 °F
Boiling Point 988 °C1810 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 3.303.30
 
Component Elements PropertiesMetricEnglishComments
Tellurium, Te 100 %100 %
 
Descriptive Properties
CAS Number13494-80-9

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Selenium, Se
Silicon, Si
Tin, Sn
Silver, Ag
Terbium, Tb

AMETe00 / 113

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.