MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Plastics TufGuard E™ XP-115D-Zeta PE, Flame Retardant
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 94
@Time 15.0 sec
94
@Time 0.00417 hour
ASTM D2240
Tensile Strength 8.62 MPa1250 psiASTM D412
 6.896 MPa
@Temperature 100 °C,
Time 346000 sec
1000 psi
@Temperature 212 °F,
Time 96.0 hour
Oil Aged
 8.3614 MPa
@Temperature 121 °C,
Time 605000 sec
1212.7 psi
@Temperature 250 °F,
Time 168 hour
Aged
Elongation at Break 500 %500 %ASTM D412
 450 %
@Treatment Temp. 100 °C,
Time 346000 sec
450 %
@Treatment Temp. 212 °F,
Time 96.0 hour
Oil Aged
 515 %
@Treatment Temp. 121 °C,
Time 605000 sec
515 %
@Treatment Temp. 250 °F,
Time 168 hour
Aged
100% Modulus 5.86 MPa
@Strain 100 %
850 psi
@Strain 100 %
STM D412
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= 50.0 °C<= 122 °FASTM D746
Oxygen Index >= 27 %>= 27 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aurora Plastics CPE-01-266A-405 Black CPE
Aurora Plastics TufGuard E™ XP-115DD-Zeta PE, Flame Retardant
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin

PSEPN115 / 179119

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.