MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Plastics CPE-01-266A-405 Black CPE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Application: 90° C, oil resistant CPE based, FT4, 210,000 BTU wire and cable jacketing material with enhanced tear properties and flexibility.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 - 1.41 g/cc1.35 - 1.41 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 90 - 9590 - 95ASTM D2240
Tensile Strength 12.4 MPa1800 psiASTM D412
 13.46 MPa
@Treatment Temp. 121 °C,
Time 605000 sec
1952 psi
@Treatment Temp. 250 °F,
Time 168 hour
Air Oven aged; UL1581
Elongation at Break 325 %325 %ASTM D412
 390 %
@Treatment Temp. 121 °C,
Time 605000 sec
390 %
@Treatment Temp. 250 °F,
Time 168 hour
Air Oven aged; UL1581
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -16.0 °C<= 3.20 °FASTM D746
Oxygen Index 36 %36 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aurora Plastics CPE-01-266LT Wire and Cable CPE
Aurora Plastics TufGuard E™ XP-115D-Zeta PE, Flame Retardant
Aurora Plastics TufGuard E™ XP-115DD-Zeta PE, Flame Retardant
BorsodChem ONGRO CPE 3602 N Chlorinated Polyethylene
Ethylene Propylene Rubber (EPM, EPDM)

PSEPO012 / 140975

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.