Homopolymer Applications: Totes, cases, crates, over-caps, toys Formolene LH6008 is a high density polyethylene for injection molding applications. Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact. Information provided by Formosa Plastics Corporation, USA. |