System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Injection Molded
Material Notes:
Data Provided by Exxon Chemical Canada.
Characteristics: High Flow, Good Stiffness
Uses: Food containers, Small pails, Nursery containers
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.951
g/cc
0.0344
lb/in³
ASTM D4883
ESCR 10% Igepal®
<=
2.0
hour
<=
2.0
hour
F-50; Cond. B; ASTM D-1693
Linear Mold Shrinkage
0.016
cm/cm
0.016
in/in
Exxon Method
Melt Flow
33
g/10 min
@Load 2.16 kg,
Temperature 190 °C
33
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow
55.8
cm
22.0
in
Exxon Method
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
22.1
MPa
3210
psi
ASTM D638
Elongation at Yield
20 %
20 %
ASTM D638
Flexural Modulus
0.558
GPa
80.9
ksi
ASTM D790
Thermal Properties
Metric
English
Comments
Melting Point
130
°C
266
°F
Exxon Method
Brittleness Temperature
<=
-70.0
°C
<=
-94.0
°F
ASTM D746
Processing Properties
Metric
English
Comments
Nozzle Temperature
260
°C
500
°F
Nozzle (Melt)
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade
ExxonMobil HD 50330 High Density Polyethylene Copolymer Resin
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
ExxonMobil Escorene® HD-6705 HDPE, Injection Grade
PEXCA8 / 37827
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.