MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Akrochem PROAID® PEP Process Aids
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Proaid PEP is a mixture of zinc salts of high molecular weight fatty acids. It can be used as a processing aid and for natural and synthetic rubber. It provides excellent mill release in epichlorohydrin compounds.

Applications: The dosage for Proaid PEP is 2 to 5 phr, depending on the polymer and the process. Proaid PEP may be used:

  • To obtain lower power consumption during the mixing cycle
  • To obtain lower dumping temperature
  • To obtain lower mooney viscosity
  • To improve vulcanization uniformity
  • To improve filler dispersion in dry compounds
  • To aid blending of elastomers

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Ash <= 15 %
@Temperature 800 °C
<= 15 %
@Temperature 1470 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 205 - 216 °C401 - 421 °F
 
Descriptive Properties
Appearanceivory-colored pastilles
Content0.02Free ZnO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH365 / 315283

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.