Product Description: Proaid PEP is a mixture of zinc salts of high molecular weight fatty acids. It can be used as a processing aid and for natural and synthetic rubber. It provides excellent mill release in epichlorohydrin compounds. Applications: The dosage for Proaid PEP is 2 to 5 phr, depending on the polymer and the process. Proaid PEP may be used: - To obtain lower power consumption during the mixing cycle
- To obtain lower dumping temperature
- To obtain lower mooney viscosity
- To improve vulcanization uniformity
- To improve filler dispersion in dry compounds
- To aid blending of elastomers
Information provided by Akrochem Corporation |