Temper: As Continuous Cast Casting Characteristics: High – Casting Yield, Effect of Section Size; Medium – Fluidity, Gassing, Shrinkage in Solidification; Low - Drossing Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing; Fair Suitability – Coated Metal Arc Welding Typical uses: Hardware; Electrical Components; Switches; Air-Gas-Water Fittings; Bushings; Pump Fixtures; Railroad Catenary Fittings; Valves; Plumbing Fixtures Applicable Specifications: As Centrifugal Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B271/B271M; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings SAE J462, Castings ASTM B584, Castings SAE J461, Castings B763/B763M; Fitting – ASTM B584, ASME B16.32, ASME B16.23, ASME B16.18, ASME B16.15; Ingot - ASTM B30; Unions – FEDERAL WW-U-516 |