MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hydraulic Bronze, UNS C83800, M07 Temper, As Continuous Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Continuous Cast

Casting Characteristics: High – Casting Yield, Effect of Section Size; Medium – Fluidity, Gassing, Shrinkage in Solidification; Low - Drossing

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing; Fair Suitability – Coated Metal Arc Welding

Typical uses: Hardware; Electrical Components; Switches; Air-Gas-Water Fittings; Bushings; Pump Fixtures; Railroad Catenary Fittings; Valves; Plumbing Fixtures

Applicable Specifications: As Centrifugal Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B271/B271M; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings SAE J462, Castings ASTM B584, Castings SAE J461, Castings B763/B763M; Fitting – ASTM B584, ASME B16.32, ASME B16.23, ASME B16.18, ASME B16.15; Ingot - ASTM B30; Unions – FEDERAL WW-U-516

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.64 g/cc0.312 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 207 MPa>= 30000 psi
Tensile Strength, Yield >= 103 MPa>= 15000 psi
Elongation at Break >= 16 %>= 16 %
Tensile Modulus 91.7 GPa13300 ksi
Machinability 90 %90 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000115 ohm-cm0.0000115 ohm-cm15% IACS
Magnetic Permeability 1.01.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 200 °C
10.0 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 6.02 W/m-K41.8 BTU-in/hr-ft²-°F
Melting Point 843 - 1000 °C1550 - 1840 °F
Solidus 843 °C1550 °F
Liquidus 1000 °C1840 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.25 %<= 0.25 %
Copper, Cu 82 - 83.8 %82 - 83.8 %
Iron, Fe <= 0.30 %<= 0.30 %
Lead, Pb 5.0 - 7.0 %5.0 - 7.0 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.0050 %<= 0.0050 %
Sulfur, S <= 0.080 %<= 0.080 %
Tin, Sn 3.3 - 4.2 %3.3 - 4.2 %
Zinc, Zn 5.0 - 8.0 %5.0 - 8.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC83800x2 / 293146

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.