MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

AdvanSix Capran® NyLid™ WMB 175 Nylon/EVOH Lidding Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Alcohol (EVOH); Nylon (Polyamide PA)

Material Notes: Capran® NyLid™ WMB 175 is a 1.75 mil, white medium barrier nylon co-extruded film with an EVOH core.

Applications: Capran® NyLid™ WMB 175 is suitable for die cutting, readily accepts printing, accepts heal seal coatings and lacquers, offers excellent puncture resistance, is safe for microwave use, and resists tear propagation. It is ideally suited for lamination, and is FDA compliant for indirect food contact.

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0420 lb/in³Yield Density
Water Vapor Transmission 217.1 g/m²/day
@Temperature 37.8 °C
13.98 g/100 in²/day
@Temperature 100 °F
100%RH; ASTM F1249
Oxygen Transmission Rate 1.40 cc/m²/day0.0902 cc/100 in²/dayASTM D3985
Thickness 44.5 microns1.75 mil
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 34.5 MPa5000 psiASTM D882
Film Tensile Strength at Yield, TD 34.5 MPa5000 psiASTM D882
Film Elongation at Break, MD 360 %360 %ASTM D882
Film Elongation at Break, TD 370 %370 %ASTM D882
Secant Modulus, MD 1.027 GPa149.0 ksiASTM D882
Secant Modulus, TD 0.9997 GPa145.0 ksiASTM D882
Coefficient of Friction 0.210.21film to stainless steel; ASTM D1894
 0.400.40film to film; ASTM D1894
Tear Strength Test 520520graves tear MD, initial, grams/mil; ASTM D1004
 520520graves tear TD, initial, grams/mil; ASTM D1004
Elmendorf Tear Strength, MD 4.500 g/micron114.3 g/mil
Elmendorf Tear Strength, TD 6.7492 g/micron171.43 g/milpropagated; ASTM D1922
Film Tensile Strength at Break, MD 101 MPa14700 psiASTM D882
Film Tensile Strength at Break, TD 89.6 MPa13000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD -3.20 %
@Treatment Temp. 177 °C,
Time 601 sec
-3.20 %
@Treatment Temp. 350 °F,
Time 0.167 hour
ASTM D1204
Shrinkage, TD >= -0.600 %
@Treatment Temp. 177 °C,
Time 601 sec
>= -0.600 %
@Treatment Temp. 350 °F,
Time 0.167 hour
ASTM D1204
 
Optical PropertiesMetricEnglishComments
Gloss 80 %80 %at 60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AdvanSix Capran® NyLid™ WMB 250 Nylon/EVOH Lidding Film
Trinseo BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Tetrabromosilane, SiBr4
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)

PALC034 / 23796

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.