MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Estane® 58437 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).

Features: Excellent cold temperature properties and improved heat resistance.

Uses: Blown and flat die/cast film extrusion and tubing and profile extrusion.

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82 - 88
@Time 5.00 sec
ASTM D2240
Tensile Strength 42.7 MPaASTM D412
Elongation at Break 560 %ASTM D412
100% Modulus 0.00550 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.00970 GPa
@Strain 300 %
ASTM D412
Tear Strength 140 pliTrouser; ASTM D470
Graves Tear Strength 450 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 23
@Load 1.00 kg
H-18 wheel; ASTM D3389
Tensile Set 12 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 167 °CDSC
 168 °CKofler
Glass Transition Temp, Tg -40.0 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 5.4 %pressed between glass; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Zone 1 182 °CExtrusion
Zone 2 188 °CExtrusion
Zone 3 193 °CExtrusion
Zone 4 199 °CExtrusion
Adapter Temperature 199 °C5, Extrusion
Die Temperature 199 °CZone 1, 6, Extrusion
 199 °CZone 2, Extrusion
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
 
Descriptive Properties
Volume Swell in Jet fuel (JP8)4.9%24h/23°C, ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® CS195A Thermoplastic Polyurethane
Lubrizol Estane® L194A Thermoplastic Polyurethane
Lubrizol Estane® S385A Thermoplastic Polyurethane
Lubrizol ESTANE® 5799 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5735 Ester Based Thermoplastic Polyurethane

PNOVEON561 / 121452

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.