Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU). Features: Excellent cold temperature properties and improved heat resistance. Uses: Blown and flat die/cast film extrusion and tubing and profile extrusion. Information Provided by The Lubrizol Corporation |