MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aurora Plastics TufFill NH™ 2102A PP, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Application: A polypropylene based, zero halogen, flame retardant compound with antistatic properties designed for packaging applications.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Melt Flow 13 g/10 min13 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 16.5 MPa2390 psiASTM D638
Tensile Strength, Yield 23.1 MPa3350 psiASTM D638
Elongation at Break >= 58 %>= 58 %ASTM D638
Flexural Modulus 1.68 GPa244 ksitangent; ASTM D790
Izod Impact, Notched 0.587 J/cm1.10 ft-lb/inASTM D256
Dart Drop Total Energy 1.44 J/cm0.00270 ft-lb/milASTM D5420
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.50e+11 ohm1.50e+11 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® QD 818 30% Glass Fiber Reinforced Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® QD 813 Y001 WOD Flame Retardant Polypropylene
Celanese SO.F.TER Polifor® QD 813 30% Glass Fiber Reinforced Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® 5220/V0-EP Mineral Filled Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® 5220/V0 EPWOD Flame Retardant Polypropylene

PSEPN010 / 179014

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.