System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Aurora Plastics TufFill NH™ 2102A PP, Flame Retardant
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Flame Retardant
Material Notes:
Application: A polypropylene based, zero halogen, flame retardant compound with antistatic properties designed for packaging applications.
Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.06
g/cc
ASTM D792
Melt Flow
13
g/10 min
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
2390
psi
ASTM D638
Tensile Strength, Yield
3350
psi
ASTM D638
Elongation at Break
>= 58 %
ASTM D638
Flexural Modulus
1680
MPa
tangent; ASTM D790
Izod Impact, Notched
1.10
ft-lb/in
ASTM D256
Dart Drop Total Energy
1.44
J/cm
ASTM D5420
Electrical Properties
Original Value
Comments
Surface Resistance
1.50e+11
ohm
ASTM D257
Thermal Properties
Original Value
Comments
Flammability, UL94
V-0
@Thickness 1.59 mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® QD 818 30% Glass Fiber Reinforced Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® QD 813 Y001 WOD Flame Retardant Polypropylene
Celanese SO.F.TER Polifor® QD 813 30% Glass Fiber Reinforced Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® 5220/V0-EP Mineral Filled Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® 5220/V0 EPWOD Flame Retardant Polypropylene
PSEPN010 / 179014
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.