MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Huntsman AVALON® 98 AE Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling material for sports footwear and top-pieces. The features offered include:
  • Durability
  • Excellent surface definition
  • Abrasion resistance
  • Flex resistance
  • Phthalate free TPU

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9898ISO 868
Hardness, Shore D 5656ISO 868
Tensile Strength at Break 34.0 MPa4930 psiISO 37
Elongation at Break 350 %350 %ISO 37
100% Modulus 16.0 MPa
@Strain 100 %
2320 psi
@Strain 100 %
ISO 37
300% Modulus 24.0 MPa
@Strain 300 %
3480 psi
@Strain 300 %
ISO 37
Tear Strength 165 kN/m941 pliISO 34B
Abrasion 3535mm3; ISO 4649
Compression Set 20 %20 %ISO 815
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 35.0 °C77.0 - 95.0 °F
Rear Barrel Temperature 185 - 195 °C365 - 383 °F
Middle Barrel Temperature 190 - 200 °C374 - 392 °F
Front Barrel Temperature 195 - 205 °C383 - 401 °F
Nozzle Temperature 180 - 190 °C356 - 374 °F
Mold Temperature 25.0 - 50.0 °C77.0 - 122 °F
Injection Pressure 2.00 - 10.0 MPa290 - 1450 psi
Hold Pressure 1.00 - 5.00 MPa145 - 725 psi
Back Pressure 0.0300 - 0.300 MPa4.35 - 43.5 psi
Screw Speed 20 - 80 rpm20 - 80 rpm
 
Descriptive Properties
Compression Ratio2-3:1
L/D Ratio20-25:1
Ross Flex-10°C, BS 5131
Typical Screw Diameter40-120 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman AVALON® 65 DB Thermoplastic Polyurethane
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
LG Chemical LUPOL GP1000FC Flame Retardant PP
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether
Huntsman AVALON® 98 AB Thermoplastic Polyurethane

PHUQ164 / 159537

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.