MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Pressure Seal 22701 Ethylene - Acrylic
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Compound 22701 is a 70 durometer black colored Ethylene - Acrylic (Vamac®) elastomer. It exhibits excellent resistance to heat, water and compression set. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 4 EE 715 A47 B46 B37 EO16 EO36 EA14 G21; 3 EE 712 A47 B46 B37 EO16 EO36 EA14 G21; 5 EE 712 A47 B46 B37 EO16 EO36 EA14 G21

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
 58
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 71
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 72
@Treatment Temp. 100 °C,
Time 252000 sec
Distilled water aged
 75
@Treatment Temp. 175 °C,
Time 252000 sec
Heat Aged
 77
@Treatment Temp. 175 °C,
Time 605000 sec
Heat Aged
Tensile Strength 2482 psi
 1662.9 psi
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 2454.7 psi
@Treatment Temp. 175 °C,
Time 252000 sec
Heat Aged
 2516.7 psi
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 2558.9 psi
@Treatment Temp. 175 °C,
Time 605000 sec
Heat Aged
Elongation, Ultimate 235 %
 184.9 %
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 224 %
@Treatment Temp. 175 °C,
Time 252000 sec
Heat Aged
 224.9 %
@Treatment Temp. 175 °C,
Time 605000 sec
Heat Aged
 241.1 %
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
50% Modulus 428 psi
100% Modulus 1047 psi
Tear Strength 205 pliDie C
 260 pliDie B
Compression Set 5.0 %
@Treatment Temp. 175 °C,
Time 79200 sec
Solid
 6.7 %
@Treatment Temp. 150 °C,
Time 79200 sec
Plied
 6.8 %
@Treatment Temp. 175 °C,
Time 79200 sec
Plied
 7.4 %
@Treatment Temp. 150 °C,
Time 79200 sec
Solid
 9.9 %
@Treatment Temp. 175 °C,
Time 252000 sec
Solid
 12.2 %
@Treatment Temp. 175 °C,
Time 252000 sec
Plied
 13.1 %
@Treatment Temp. 150 °C,
Time 252000 sec
Solid
 15.5 %
@Treatment Temp. 150 °C,
Time 252000 sec
Plied
 31.7 %
@Treatment Temp. 150 °C,
Time 2.59e+6 sec
Solid
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -35.0 °F
Shrinkage 3.1 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, Distilled water aged
 7.4 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 48.5 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 
Descriptive Properties
ColorBlack
TR-10 Temperature-26°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL218 / 318428

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.