Description: This is a two-component, 100% silicone solids, thermally conductive elastomer designed for electronic potting and roller applications. Key Features - Flame retardant
- High thermal conductivity
- Low viscosity
- Electrically insulating
Application: TIM gap fillerInformation provided by CHT Group |