MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

CHT SilSo Cool 21311 Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a two-component, 100% silicone solids, thermally conductive elastomer designed for electronic potting and roller applications.

Key Features

  • Flame retardant
  • High thermal conductivity
  • Low viscosity
  • Electrically insulating
Application: TIM gap filler

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.82 g/cc0.102 lb/in³A; BS ISO 2781
 2.82 g/cc0.102 lb/in³B; BS ISO 2781
Brookfield Viscosity 22000 cP22000 cPB
 23000 cP23000 cPMixed
 23900 cP23900 cPA
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545ASTM D2240-95
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.80e+14 ohm-cm3.80e+14 ohm-cmASTM D-257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.30 W/m-K16.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life >= 50.0 min>= 50.0 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceViscous liquid
ColorGreyB
 GreyCured Product
 Off whiteA
Mix Ratio1:1By Weight
Self BondingNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL070 / 314553

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.