Temper: As Centrifugal Cast Casting Characteristics: High – Fluidity, Gassing; Medium – Shrinkage in Solidification, Casting Yield, Effect of Section Size; Low – Drossing Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding; Good Suitability - Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld; Fair Suitability – Oxyacetylene Welding Typical uses: Artistry Components, Electrical Components, Bearings, Engineering Applications, Valve Bodies Applicable Specifications: As Centrifugal Cast - Castings ASTM B271/B271M; As Sand Cast – Castings ASTM B584, Castings ASTM B763/B763M; Ingot - ASTM B30 |