MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Low-Zinc Silicon Brass, UNS C87600, Copper Casting Alloy, M02 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: As Centrifugal Cast

Casting Characteristics: High – Fluidity, Gassing; Medium – Shrinkage in Solidification, Casting Yield, Effect of Section Size; Low – Drossing

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding; Good Suitability - Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld; Fair Suitability – Oxyacetylene Welding

Typical uses: Artistry Components, Electrical Components, Bearings, Engineering Applications, Valve Bodies

Applicable Specifications: As Centrifugal Cast - Castings ASTM B271/B271M; As Sand Cast – Castings ASTM B584, Castings ASTM B763/B763M; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.30 g/cc0.300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 414 MPa>= 60000 psifor Standard
Tensile Strength, Yield >= 207 MPa>= 30000 psifor Standard, 0.5% Ext
Elongation at Break >= 16 %>= 16 %for Standard
Tensile Modulus 117 GPa17000 ksi
Machinability 40 %40 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000290 ohm-cm0.0000290 ohm-cm6% IACS
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 2.36 W/m-K16.4 BTU-in/hr-ft²-°F
Melting Point 860 - 971 °C1580 - 1780 °F
Solidus 860 °C1580 °F
Liquidus 971 °C1780 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 88 %>= 88 %
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb <= 0.090 %<= 0.090 %
Manganese, Mn <= 0.25 %<= 0.25 %
Silicon, Si 3.5 - 5.5 %3.5 - 5.5 %
Zinc, Zn 4.0 - 7.0 %4.0 - 7.0 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC87600x1 / 293180

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.