PLA-L is a blend of polylactide, some lignin, natural fatty acids and waxes. It combines good mechanical properties comparable with ABS, high rigidity, a tensile module of elasticity of up to 397 kpsi, good impact strength down to -22°F, good resistance to polar solvents, good thermal insulation and is approved for use with foodstuffs and toys.Information provided by GEHR Plastics, Inc. |