MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GEHR Plastics ECO-GEHR® PLA-LF Polylactic Acid
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an operating range from -30°c to max 60°C.

Properties:

  • Thermoplastic based on renewable raw materials
  • Preparation from environmental friendly raw materials, thus physiologically harmless
  • PLA is biodegradable
  • Disposal by composting resp. incineration. Regional regulations need to be observed.
  • Good mechanical properties similar to ABS
  • High stiffness, modulus of elasticity up to 2740 MPa
  • Good resistance to polar media
Applications:
  • Furniture industry
  • Toy industry
  • Mechanical engineering

Information provided by GEHR Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/ccISO 1183
Moisture Absorption at Equilibrium 2.0 %2.0 %ISO 62
Water Absorption at Saturation 2.0 %2.0 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7777ISO 868
Ball Indentation Hardness 105 MPa15200 psiISO 2039
Tensile Strength at Break 33.0 MPa4790 psiISO 527
Tensile Strength, Yield 37.0 MPa5370 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Elongation at Yield 2.0 %2.0 %ISO 527
Modulus of Elasticity 2.80 GPa406 ksiISO 527
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C66.7 µin/in-°FISO 11359
Melting Point 120 °C248 °FDIN EN ISO 3146
Maximum Service Temperature, Air 60.0 °C140 °FUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C133 °FISO 75
Vicat Softening Point 57.0 °C135 °FVST/B/50; ISO 306
Glass Transition Temp, Tg 120 °C248 °FDIN EN ISO 3146
 
Compliance PropertiesMetricEnglishComments
FDA YesYesPhysiological indifference
 
Descriptive Properties
Bondabilityyes
Colornatural
Physiological indifferenceyes, EEC
UV Stabilizationno

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
GEHR Plastics ECOGEHR® PLA-L Polylactic Acid
GEHR Plastics ECOGEHR® PLA-N Polylactic Acid
LATI Latigea B01 F1 Bio-Polymer
Silicon Nitride

PGEHR041_a / 150410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.