MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lehvoss LUVOSINT® PP 9703 L WT Polypropylene copolymer for Additive Manufacturing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Polypropylene-copolymer Powder, white

Main features: Powder for laser sintering (additive manufacturing). 3D-printing of light-weight parts with high toughness for automotive, robotics and many more applications. Suitable for parts in contact with food.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/ccISO 1183-3
Water Absorption <= 0.200 %
@Time 86400 sec
<= 0.200 %
@Time 24.0 hour
ISO 62
Particle Size 25.0 µm25.0 µmPowder d10
 65.0 µm65.0 µmPowder d50
 115 µm115 µmPowder d90
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 23.0 MPa3340 psi50 mm/min; ISO 527
Elongation at Break 11.7 %11.7 %50 mm/min, Fmax; ISO 527
 269 %269 %50 mm/min; ISO 527
Tensile Modulus 0.800 GPa116 ksi1 mm/min; ISO 527
Charpy Impact Unnotched 0.470 J/cm²2.24 ft-lb/in²80x10x4mm; ISO 179 1eU
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+11 ohm<= 1.00e+11 ohmRonde 60x4mm; DIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 149 °C300 °Fmolded sample, DSC; ISO 11357
Vicat Softening Point 118 °C244 °FVST A; DIN ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8735 / 325119

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.