Polypropylene-copolymer Powder, white Main features: Powder for laser sintering (additive manufacturing). 3D-printing of light-weight parts with high toughness for automotive, robotics and many more applications. Suitable for parts in contact with food. Information provided by Lehmann & Voss & Co.KG |