MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Superior Flux Superior Supersafe® No. 30 VOC-free Organic Acid Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Formulated for electronic, electrical, industrial, artisan, and aerospace applications, including:
    • Printed Circuit Boards (PCBs)
    • Wire, Cable, and Terminal Lead Tinning and Soldering
    • Flat and Round Wire Fabrication
    • Semiconductor and Component Lead Tinning
    • Stained Glass
    • Used for Copper, Beryllium-Copper, Nickel, Alloy 42, Alloy 51, Brass, and some steels.
    • VOC-Free formulation is non-hazardous and environmentally friendly.
    • Conforms to IPC ANSI J-STD-004, Type ORM1.
    • Broad activity range an excellent choice for Tin/Lead, Tin/Silver, Tin/Bismuth, and Indium solder alloys.
    Description: Superior Supersafe® No. 30 contains an amino acid-halide activator which starts to clean metals at room temperature, reaching peak fluxing activity at 260°C/500°F, where it promotes excellent solderability. The broad range of activity makes Superior Supersafe® No. 30 an ideal choice for high production rates or difficult metal surface conditions where an active, but safe, flux is required.

    Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 - 1.05 g/cc1.03 - 1.05 g/cc
Density 1.04 g/cc0.0375 lb/in³
Solids Content 12.15 %12.15 %
pH 0.75 - 1.50.75 - 1.5
Surface Tension 35 dynes/cm35 dynes/cm
 
Processing PropertiesMetricEnglishComments
Processing Temperature 95.0 - 315 °C203 - 599 °FSoldering Range
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
Acid Equivalent0.6-1 gH+/liter
Chloride Content12.5-17.5gChlorine/liter
FormClear Blue Liquid
ResiduesCompletely Water Soluble
Spread Factor>80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nichrome 60-15 Medium Temperature Resistor Material
Tropical Balsa Wood
American Yellow Poplar Wood
American White Oak Wood
American Red Oak Wood

NSFLUX013 / 185697

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.