MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.

Applications: Bynel® 3101, 3120, and E326 adhere to a wide variety of materials. They are most often used to adhere to PE, acid copolymers, and ionomers. In addition, Bynel® 3101 and Bynel® 3120 bond to PVDC. Bynel® 3101 is also useful in adhering to polyester. Bynel® E326 also bonds to paper. The use of Bynel® Series 3100 resins can be advantageous in applications where acid-containing polymers, such as acid copolymers or ionomers, are to be combined with PVDC. Bynel® 3101, 3120, and E326 can be used in coextrusion processes including: blown film, cast film/sheet, extrusion coating, thermal lamination. Bynel® 3101 and Bynel® 3120 can also be used in blow molding.

Physical properties of Bynel® Series 3100 resins are typical of EVA resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.926 g/ccASTM D792
Viscosity 500000 cP
@Shear Rate 50 1/s,
Temperature 190 °C
Melt Flow 8.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Melting Point 67.0 °CFreezing point via DSC/ASTM D3418
 87.0 °CMelting point via DSC/ASTM D3418
Vicat Softening Point 60.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 235 °CExtruder forward zone and adapter. Degrades above 238°C.
Nozzle Temperature 235 °CDie

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDUPBI / 33563

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.