MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Fluorseals PTFE Unfilled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes:

Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.15 - 2.18 g/cc0.0777 - 0.0788 lb/in³DIN 53479
Deformation 14 %14 %14 MPa, 100 h, 23°C; ASTM D621-59
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 5955 - 59DIN 53505
Ball Indentation Hardness 27.0 - 32.0 MPa3920 - 4640 psiDIN 53456
Tensile Strength at Break 20.0 - 40.0 MPa2900 - 5800 psiASTM 1457-69 T
Elongation at Break 250 - 500 %250 - 500 %ASTM 1457-69 T
Tensile Modulus 0.750 GPa109 ksiDIN 53457
Flexural Strength 14.0 MPa2030 psi3.5% Flexural Stress; DIN 53452
Compressive Yield Strength 10.0 MPa1450 psi1% Yield Point; DIN 53454
 18.0 MPa2610 psi10% Yield Point; DIN 53454
Izod Impact, Notched (ISO) 16.0 kJ/m²7.61 ft-lb/in²DIN EN ISO 197 397
Izod Impact, Unnotched (ISO) NBNBDIN EN ISO 197 397
Coefficient of Friction, Dynamic 0.23 - 0.270.23 - 0.27v = 1 m/s
 0.25 - 0.280.25 - 0.28v = 1.9 m/s
Abrasion 4.04.0mm of depth after 5 hrs load duration; Partner Material ST 50
Torsional Stiffness 160 MPa23200 psiDIN 53447
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+18 ohm-cm1.00e+18 ohm-cmDIN 53482
Surface Resistance 1.00e+17 ohm1.00e+17 ohmDIN 53482
Dielectric Constant 2.1
@Frequency 50.0 - 100 Hz
2.1
@Frequency 50.0 - 100 Hz
DIN 53483
Dielectric Strength 50.0 - 80.0 kV/mm
@Thickness 0.200 mm
1270 - 2030 kV/in
@Thickness 0.00787 in
VDE 0303 Part 2
Dissipation Factor  0.000030
@Frequency 1000 Hz
0.000030
@Frequency 1000 Hz
DIN 53483
 0.000050
@Frequency 50 Hz
0.000050
@Frequency 50 Hz
DIN 53483
 0.000070
@Frequency 1e+6 Hz
0.000070
@Frequency 1e+6 Hz
DIN 53483
 <= 0.00010
@Frequency 1000 - 100000 Hz,
Temperature -50.0 - 200 °C
<= 0.00010
@Frequency 1000 - 100000 Hz,
Temperature -58.0 - 392 °F
DIN 53483
Comparative Tracking Index >= 600 V>= 600 VVDE 0303 Part 1/9.64
 
Thermal PropertiesMetricEnglishComments
CTE, linear  160 µm/m-°C
@Temperature 20.0 - 100 °C
88.9 µin/in-°F
@Temperature 68.0 - 212 °F
DIN 52328
 195 µm/m-°C
@Temperature 20.0 - 200 °C
108 µin/in-°F
@Temperature 68.0 - 392 °F
DIN 52328
 250 µm/m-°C
@Temperature 20.0 - 300 °C
139 µin/in-°F
@Temperature 68.0 - 572 °F
DIN 52328
Specific Heat Capacity  0.960 J/g-°C
@Temperature 0.000 °C
0.229 BTU/lb-°F
@Temperature 32.0 °F
adiabatic calorimeter
 1.03 J/g-°C
@Temperature 50.0 °C
0.246 BTU/lb-°F
@Temperature 122 °F
adiabatic calorimeter
Thermal Conductivity >= 0.500 W/m-K>= 3.47 BTU-in/hr-ft²-°FDIN 52612
Melting Point 320 - 340 °C608 - 644 °FMelting Range; DTA
Maximum Service Temperature, Air 260 °C500 °FLong Term
 300 °C572 °FShort Term
Vicat Softening Point 110 °C230 °Fin air; DIN 53460
Minimum Service Temperature, Air -200 °C-328 °F
 
Descriptive Properties
Bending cycles to failure>10^6
Heat of Combustion4600 kJ/kg
Incandescence resistanceLevel 1
Volume change between r.t. and melting range27 to 28%
Volume Change in the melting interval5 to 8%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SP-211 Polyimide, 15% Graphite, 10% Teflon® Filled, Machined
AGC Fluon® PTFE
Overview of materials for Polyetheretherketone, Unreinforced
DuPont Mobility and Materials Vespel® SF-0940 Polyimide Foam, High Density
Ensinger TECASINT 1611 Polyimide, 30% PTFE Filled (PI)

PTEKU0 / 70053

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.