MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta RT504 Phenolic Fiber Glass Laminate Tube, NEMA G-3
Categories: Polymer; Thermoset; Phenolic

Material Notes: RT504 is a heavy weave glass fabric combined with a phenolic resin system. It has excellent heat and chemical resistance in basic systems. It has good physical strength and high impact resistance. Typical applications include structural parts and can be substituted for G-7 in certain applications.

Information provided by Norplex-Micarta

Key Words: Fiber Glass, Phenolic, NEMA G-3
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/cc0.750" X 1.000"; ASTM D792
Moisture Absorption 0.200 %0.200 %0.750" X 1.000"; ASTM D570 Condition D1-24/23
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 1051050.750" X 1.000"; ASTM D785
Tensile Strength 265 MPa38500 psi0.750" X 1.000"; ASTM D638 Condition A
Compressive Strength 262 MPa38000 psi0.750" X 1.000"; ASTM D695 Condition A
Compressive Modulus 5.86 GPa850 ksi0.750" X 1.000"; ASTM D695 Condition A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.8 kV/mm350 kV/in0.750" X 1.000"; ASTM D149 Condition D-48/50
 15.7 kV/mm400 kV/in0.750" X 1.000"; ASTM D149 Condition A
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 180 °C356 °F0.750" X 1.000"; UL Bulletin 746b
UL RTI, Mechanical with Impact 160 °C320 °F0.750" X 1.000"; UL Bulletin 746b
Flammability, UL94 HBHB0.750" X 1.000"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta RT504F Phenolic Fiber Glass Laminate Tube, NEMA G-3
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Compression Grade
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Compression Grade
Norplex-Micarta RT571 Epoxy Fiber Glass Laminate Tube, NEMA G-10
Norplex-Micarta NP610 Phenolic Paper Laminate Sheet, NEMA X

PNORPM128 / 192867

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.