MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Afton Plastics 450FC30 PEEK 30% Carbon Fiber Filled Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Afton plastics produces shapes and components from Victrex™ PEEK®, a high-performance thermoplastic that has an extraordinary combination of mechanical, structural and chemical resistance.

Product Benefits: • Wear resistance • Service temperature: -50°F to +500°F • Hydrolysis resistance • Radiation resistance • FDA compliant

Applications: Thrust washers • Pump gears • Compressor valve plates • Electrical connectors • Valve seats and seals • Bearings and bushings.

Information provided by Afton Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³Crystalline; ISO 1183
Water Absorption at Saturation 0.35 %
@Temperature 23.0 °C
0.35 %
@Temperature 73.4 °F
By immersion; ISO 62-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383
Tensile Strength at Break 150 MPa21800 psiISO 527
Elongation at Break 2.3 %2.3 %ISO 527
Flexural Strength 230 MPa33400 psiISO 178
Flexural Modulus 11.5 GPa1670 ksiISO 178
Compressive Strength 170 MPa24700 psiISO 604
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cm1V; IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear  45.0 µm/m-°C
@Temperature <=143 °C
25.0 µin/in-°F
@Temperature <=289 °F
 115 µm/m-°C
@Temperature >=143 °C
63.9 µin/in-°F
@Temperature >=289 °F
Thermal Conductivity 0.850 W/m-K5.90 BTU-in/hr-ft²-°FISO 22007-4
 0.850 W/m-K5.90 BTU-in/hr-ft²-°FISO 22007-4
Melting Point >= 343 °C>= 649 °FISO 11357
Maximum Service Temperature, Air 250 °C482 °Fcontinuous
Deflection Temperature at 1.8 MPa (264 psi) 315 °C599 °FISO 75-f
Minimum Service Temperature, Air -45.6 °C-50.0 °F
Glass Transition Temp, Tg 143 °C289 °F
Flammability, UL94 V-0V-0
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
Overview of materials for Polyetheretherketone, PTFE Filled
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Akro-Plastic Akrotek® PEEK CF 30 black (5049) PEEK, Dry, 30% Carbon Filled

PAFTON914 / 232139

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.