MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Vistalon™ 785 EPDM Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Vistalon 785 EPDM rubber is a low Mooney viscosity,  low ethylene content amorphous copolymer of ethylene and propylene with a narrow molecular weight distribution  This product is sold in dense bale form. 

Availability:  Africa & Middle East, Europe, North America, Asia Pacific, Latin America.

Vistalon™ ethylene propylene diene (EPDM) rubber grades are used in a wide variety of applications in the automotive, consumer and industrial sectors. They deliver heat-resistant part performance and processing benefits that exceed those provided by natural and general-purpose rubbers.  Benefits:  Ozone and UV resistance, Water and polar fluid resistance, Heat resistance up to 175°C, Low temperature flexibility, Elastic properties under compression, Excellent physical properties at high filler loadings, Outstanding electrical insulation.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 30
@Temperature 125 °C
30
@Temperature 257 °F
ML 1+4. Radial cavity, polymer remassed at 145°C; ASTM D1646
 
Descriptive Properties
Ethylene Content (%wt)49ASTM D3900A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Melos® FM 976 Ethylene-Propylene Diene Elastomer (EPDM) Compound
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600
Garlock 8314 EPDM Sheet Rubber Gasketing
Garlock 563 EPDM Sheet Rubber
Evonik Solimide® TA-301-DODI Polyimide Foam

PEX98818 / 238203

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.