MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals NOVAPOL® HB-L354-A HDPE Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes:

Hexene Copolymer

Features:

  • Good balance of physical and molding properties; high toughness
  • Excellent processability on high-speed, multiple-head blow molding lines
  • UL 94 HB

Additives:

  • Process stabilizer

Applications:

  • Household chemical bottles
  • Industrial chemical bottles
  • Automotive fluid bottles
  • Pharmaceutical bottles
  • Toys

United States: NOVAPOL HB-L354-A resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ASTM D 792
ESCR 100% Igepal® 48 hour48 hourF50, Condition B; ASTM D 1693
Melt Index of Compound 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 31.0 MPa4500 psiASTM D 638
Elongation at Break 900 %900 %ASTM D 638
Flexural Modulus 1.18 GPa171 ksiASTM D790
Izod Impact, Unnotched 2.70 J/cm
@Thickness 3.20 mm
5.06 ft-lb/in
@Thickness 0.126 in
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 125 °C257 °FASTM D 1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HD 9856B Blow Molding Resin
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)
Dow DMDB-7950 NT 7 High Density Polyethylene Resin
ExxonMobil HD 5705 High Density Polyethylene Resin
Overview of materials for High Density Polyethylene (HDPE), Extruded

PNOVB009 / 194617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.