MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DMDB-7950 NT 7 High Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short molding cycles.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ASTM D792
ESCR 100% Igepal® 40 hour
@Temperature 50.0 °C
40 hour
@Temperature 122 °F
F50; Molded and tested in accordance with ASTM D4976; ASTM D1693
Melt Index of Compound 5.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5454Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 26.2 MPa3800 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 24.8 MPa3600 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 1200 %1200 %Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 8.0 %8.0 %Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 1.01 GPa
@Strain 2 %
146 ksi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength 105 kJ/m²50.0 ft-lb/in²Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FDow Method (DSC)
Crystallization Temperature 118 °C244 °FDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 67.8 °C154 °FMolded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FMolded and tested in accordance with ASTM D4976; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DMDA-8907 NT 7 High Density Polyethylene Resin
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
Dow DMDA-8965 NT 7 High Density Polyethylene Resin
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin
Dow DMDA-8904 NT 7 High Density Polyethylene Resin

PDOW1267 / 30485

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.