MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teijin Tenax® E TPWF PEEK-HTA40 Composite
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes:
  • High-performance mechanical properties
  • Continuous use at elevated temperature
  • Low flammability, smoke and toxicity
  • Resistant to chemicals and solvents
  • Room temperature storage and shipping
  • Compliant to Health, Safety and Environment requirement
  • Recyclable
Process Benefits
  • Out of autoclave consolidation (press forming, vacuum bagging)
  • Short cycle time
  • Thermo-formable
  • Thermoplastic joining technologies (molded sheet form)

Information provided by Teijin Carbon America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.77 g/cc0.0639 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 320 MPa46400 psiOpen Hole (0°), [((0,90)/ (+45,-45))3]s; European
 347.2 MPa50350 psiFilled Hole (0°), [((0,90)/ (+45,-45))3]s; European
 647 MPa93800 psiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 908.7 MPa131800 psiweft, Stacking Sequence: [(0,90)3]s; ISO 527-4 type 3
 954.9 MPa138500 psiwarp, Stacking Sequence: [(0,90)3]s; ISO 527-4 type 3
Tensile Modulus 42.0 GPa6090 ksiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 60.0 GPa8700 ksiwarp, Stacking Sequence: [(0,90)3]s; ISO 527-4 type 3
 60.0 GPa8700 ksiweft, Stacking Sequence: [(0,90)3]s; ISO 527-4 type 3
Flexural Strength 1225 MPa177700 psiwarp, Stacking Sequence: [(0,90)3]s; EN 2562 A
 1058 MPa
@Temperature 90.0 °C
153400 psi
@Temperature 194 °F
warp, Stacking Sequence: [(0,90)3]s; EN 2562 A
Flexural Modulus 66.2 GPa9600 ksiwarp, Stacking Sequence: [(0,90)3]s; EN 2562 A
 64.8 GPa
@Temperature 70.0 °C
9400 ksi
@Temperature 158 °F
warp, Stacking Sequence: [(0,90)3]s, 85% RH; EN 2562 A
Compressive Strength 296 MPa42900 psiOpen Hole (0°), [((0,90)/ (+45,-45))3]s; European
 456.2 MPa66170 psiOpen Hole (0°), [((0,90)/ (+45,-45))3]s; European
 512 MPa74300 psiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 712.2 MPa103300 psiweft, Stacking Sequence: [(0,90)3]s; EN 2850 B2
 725.3 MPa105200 psiwarp, Stacking Sequence: [(0,90)3]s; EN 2850 B2
 266 MPa
@Temperature 90.0 °C
38600 psi
@Temperature 194 °F
Open Hole (0°), [((0,90)/ (+45,-45))3]s; European
 413 MPa
@Temperature 90.0 °C
59900 psi
@Temperature 194 °F
Plain (0°), [((0,90)/ (+45,-45))3]s; European
 414.2 MPa
@Temperature 90.0 °C
60070 psi
@Temperature 194 °F
Open Hole (0°), [((0,90)/ (+45,-45))3]s; European
Compressive Modulus 40.7 GPa5900 ksiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 40.7 GPa5900 ksiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 57.9 GPa8400 ksiweft, Stacking Sequence: [(0,90)3]s; EN 2850 B1
 59.3 GPa8600 ksiwarp, Stacking Sequence: [(0,90)3]s; EN 2850 B1
Ultimate Bearing Strength 776.3 MPa112600 psi(0°), [((0,90)/ (+45,-45))3]s; European
 864.40 MPa125370 psi(0°), [((0,90)/ (+45,-45))3]s; European
 818.34 MPa
@Temperature 70.0 °C
118690 psi
@Temperature 158 °F
(0°), [((0,90)/ (+45,-45))3]s, 85% r.h; European
Bearing Yield Strength 782.35 MPa
@Strain 2 %
113470 psi
@Strain 2 %
(0°), [((0,90)/ (+45,-45))3]s; European
 639.3 MPa
@Strain 2 %,
Temperature 90.0 °C
92720 psi
@Strain 2 %,
Temperature 194 °F
(0°), [((0,90)/ (+45,-45))3]s; European
 711.33 MPa
@Strain 2 %,
Temperature 70.0 °C
103170 psi
@Strain 2 %,
Temperature 158 °F
(0°), [((0,90)/ (+45,-45))3]s; European
Shear Modulus 5.03 GPa730 ksiIn plane, [(0,90) 2]s; European
 3.93 GPa
@Temperature 90.0 °C
570 ksi
@Temperature 194 °F
In plane, [(0,90) 2]s; European
 4.48 GPa
@Temperature 70.0 °C
650 ksi
@Temperature 158 °F
In plane, [(0,90) 2]s, 85% RH; European
Shear Strength 160 MPa23200 psiIn plane, [(0,90) 2]s; European
 121 MPa
@Temperature 90.0 °C
17500 psi
@Temperature 194 °F
In plane, [(0,90) 2]s; European
 144 MPa
@Temperature 70.0 °C
20900 psi
@Temperature 158 °F
In plane, [(0,90) 2]s; European

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEIJIN920 / 277930

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.