MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teijin Tenax® E TPWF PEEK-HTA40 Composite
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes:
  • High-performance mechanical properties
  • Continuous use at elevated temperature
  • Low flammability, smoke and toxicity
  • Resistant to chemicals and solvents
  • Room temperature storage and shipping
  • Compliant to Health, Safety and Environment requirement
  • Recyclable
Process Benefits
  • Out of autoclave consolidation (press forming, vacuum bagging)
  • Short cycle time
  • Thermo-formable
  • Thermoplastic joining technologies (molded sheet form)

Information provided by Teijin Carbon America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 46.4 ksiOpen Hole (0°), [((0,90)/ (+45,-45))3]s; European
 50.35 ksiFilled Hole (0°), [((0,90)/ (+45,-45))3]s; European
 93.8 ksiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 131.8 ksiweft, Stacking Sequence: [(0,90)3]s; ISO 527-4 type 3
 138.5 ksiwarp, Stacking Sequence: [(0,90)3]s; ISO 527-4 type 3
Tensile Modulus 6090 ksiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 8700 ksiwarp, Stacking Sequence: [(0,90)3]s; ISO 527-4 type 3
 8700 ksiweft, Stacking Sequence: [(0,90)3]s; ISO 527-4 type 3
Flexural Strength 177.7 ksiwarp, Stacking Sequence: [(0,90)3]s; EN 2562 A
 153.4 ksi
@Temperature 90.0 °C
warp, Stacking Sequence: [(0,90)3]s; EN 2562 A
Flexural Modulus 9600 ksiwarp, Stacking Sequence: [(0,90)3]s; EN 2562 A
 9400 ksi
@Temperature 70.0 °C
warp, Stacking Sequence: [(0,90)3]s, 85% RH; EN 2562 A
Compressive Strength 42.9 ksiOpen Hole (0°), [((0,90)/ (+45,-45))3]s; European
 66.17 ksiOpen Hole (0°), [((0,90)/ (+45,-45))3]s; European
 74.3 ksiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 103.3 ksiweft, Stacking Sequence: [(0,90)3]s; EN 2850 B2
 105.2 ksiwarp, Stacking Sequence: [(0,90)3]s; EN 2850 B2
 38.6 ksi
@Temperature 90.0 °C
Open Hole (0°), [((0,90)/ (+45,-45))3]s; European
 59.9 ksi
@Temperature 90.0 °C
Plain (0°), [((0,90)/ (+45,-45))3]s; European
 60.07 ksi
@Temperature 90.0 °C
Open Hole (0°), [((0,90)/ (+45,-45))3]s; European
Compressive Modulus 5900 ksiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 5900 ksiPlain (0°), [((0,90)/ (+45,-45))3]s; European
 8400 ksiweft, Stacking Sequence: [(0,90)3]s; EN 2850 B1
 8600 ksiwarp, Stacking Sequence: [(0,90)3]s; EN 2850 B1
Ultimate Bearing Strength 112600 psi(0°), [((0,90)/ (+45,-45))3]s; European
 125370 psi(0°), [((0,90)/ (+45,-45))3]s; European
 118690 psi
@Temperature 70.0 °C
(0°), [((0,90)/ (+45,-45))3]s, 85% r.h; European
Bearing Yield Strength 113470 psi
@Strain 2 %
(0°), [((0,90)/ (+45,-45))3]s; European
 92720 psi
@Strain 2 %,
Temperature 90.0 °C
(0°), [((0,90)/ (+45,-45))3]s; European
 103170 psi
@Strain 2 %,
Temperature 70.0 °C
(0°), [((0,90)/ (+45,-45))3]s; European
Shear Modulus 730 ksiIn plane, [(0,90) 2]s; European
 570 ksi
@Temperature 90.0 °C
In plane, [(0,90) 2]s; European
 650 ksi
@Temperature 70.0 °C
In plane, [(0,90) 2]s, 85% RH; European
Shear Strength 23.2 ksiIn plane, [(0,90) 2]s; European
 17.5 ksi
@Temperature 90.0 °C
In plane, [(0,90) 2]s; European
 20.9 ksi
@Temperature 70.0 °C
In plane, [(0,90) 2]s; European

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEIJIN920 / 277930

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.