MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems Accura® 55 Plastic for SLA® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Simulate the properties and appearance of molded ABS. For use with solid-state stereolithography (SLA®) systems.

    Applications
  • Automotive interior components
  • Short-run production parts
  • Electronic components
  • Testing of functional assemblies
  • Rigid and durable functional prototypes
  • Concept and marketing models
  • Accurate, durable master patterns for urethane casting

All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. Innovative leaders in producing high quality Rapid Prototyping and Rapid Manufacturing solutions using all major 3D printing systems including Stereolithography technology. Free online quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
@Temperature 25.0 °C
Liquid
 1.20 g/cc
@Temperature 25.0 °C
Solid
Viscosity 155 - 185 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Tensile Strength, Yield 63.0 - 68.0 MPaASTM D638
Elongation at Break 5.0 - 8.0 %ASTM D638
Tensile Modulus 3200 - 3380 MPaASTM D638
Flexural Strength 88.0 - 110 MPaASTM D790
Flexural Modulus 2690 - 3240 MPaASTM D790
Izod Impact, Notched 12.0 - 22.0 J/mASTM D256
Gardner Impact 1.10 JASTM D5420
Penetration 5.2mils
 
Thermal PropertiesOriginal ValueComments
CTE, linear 61.0 µm/m-°C
@Temperature 0.000 - 40.0 °C
T
 163 µm/m-°C
@Temperature 75.0 - 140 °C
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 55.0 - 58.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 53.0 °CASTM D648
Glass Transition Temp, Tg 56.0 °CDMA, E"
 
Descriptive Properties
AppearanceWhite
Critical Exposure (mJ/cm²)7.4
Tested Build StylesFAST™, EXACT™, Exact HR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3D Systems Accura® 60 Plastic for SLA® Systems
DSM Somos® 9120
DSM Somos® PerFORM Stereolithography Polymer, Thermal Postcure
Proto3000 Objet TangoBlackPlus FullCure980 Rubber-like Prototyping Polymer
3D Systems Accura® 50 Plastic for SLA® Systems

PAPPR109 / 83488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.