MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems Accura® 50 Plastic for SLA® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.

    Applications
  • Functional components for assemblies, mock-ups and test for many uses, including:
    • Enclosures, covers and cases for consumer goods
    • Toys
    • Cellular/mobile telephones
    • Electronic components: connectors, interconnects, routing enclosures, etc.
    • Automotive design elements: dash boards, air conditioning vents, etc.
  • Accurate, durable master patterns for RTV or silicone molding
  • Limited snap-fits and assemblies
  • Simulate a molded part
  • Concept models
  • Marketing models

All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. Industry leaders in providing high quality Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including Stereolithography printing technology. Free 3D quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density  1.14 g/cc
@Temperature 25.0 °C
0.0412 lb/in³
@Temperature 77.0 °F
Liquid
 1.21 g/cc
@Temperature 25.0 °C
0.0437 lb/in³
@Temperature 77.0 °F
Solid
Viscosity 600 cP
@Temperature 30.0 °C
600 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Tensile Strength, Yield 48.0 - 50.0 MPa6960 - 7250 psiASTM D638
Elongation at Break 5.3 - 15 %5.3 - 15 %ASTM D638
Tensile Modulus 2.48 - 2.69 GPa360 - 390 ksiASTM D638
Flexural Strength 72.0 - 77.0 MPa10400 - 11200 psiASTM D790
Flexural Modulus 2.21 - 2.34 GPa321 - 339 ksiASTM D790
Izod Impact, Notched 0.165 - 0.281 J/cm0.309 - 0.526 ft-lb/inASTM D256
Penetration 4.54.5mils
 
Thermal PropertiesMetricEnglishComments
CTE, linear  73.0 µm/m-°C
@Temperature 0.000 - 20.0 °C
40.6 µin/in-°F
@Temperature 32.0 - 68.0 °F
T
 164 µm/m-°C
@Temperature 90.0 - 150 °C
91.1 µin/in-°F
@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 49.0 - 53.0 °C120 - 127 °FASTM D648
 74.0 - 80.0 °C165 - 176 °Fwith 160ºC thermal postcure; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.0 - 46.0 °C109 - 115 °FASTM D648
Glass Transition Temp, Tg 62.0 °C144 °FDMA, E"
 
Descriptive Properties
AppearanceOpaque natural or opaque grey
Critical Exposure (mJ/cm²)9
Tested Build StylesFAST™, EXACT™, Exact HR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems Accura® 55 Plastic for SLA® Systems
3D Systems DuraForm® AF Nylon for SLS® Systems
3D Systems Accura® 25 Plastic for SLA® Systems

PAPPR108 / 83487

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.