MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Acclaim® 6300 Polyol
Categories: Polymer; Thermoset

Material Notes: Characterization: Acclaim 6300 polyol is a 6,000-molecular-weight triol based on propylene oxide.

Properties / Applications: Acclaim 6300 polyol is a 6,000-molecular-weight triol based on propylene oxide. This high-performance, low-monol polyether is prepared with Covestro's proprietary IMPACT™ technology, using a patented organo-metallic propoxylation catalyst. The terminal end-groups are predominantly secondary hydroxyls and have a relatively low reactivity. This polyol is acidified with a low level of phosphoric acid, making it suitable for use in isocyanate-terminated prepolymers. Acclaim 6300 polyol is used in polyurethane and other applications, including cast elastomers, sealants, adhesives, epoxy flexibilizers, defoamers, reaction injection molding (RIM), lubricants, crude oil de-emulsifiers and plasticizers. As with any product, use of Acclaim 6300 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Acclaim 6300 polyol is a complementary product to Acclaim 4200 polyol, an ultra-low monol diol with the same equivalent weight. Overall polyol functionality can easily be varied by blending these two polyols. This polyol contains extremely low levels of monol. In some polyurethane systems, formulation changes, such as reducing the crosslinking level or changing the hard-segment content, may be necessary to maximize the benefits of using Acclaim polyols.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/cc
 0.960 g/cc
@Temperature 80.0 °C
0.960 g/cc
@Temperature 176 °F
 0.990 g/cc
@Temperature 40.0 °C
0.990 g/cc
@Temperature 104 °F
Bulk Density 1.01 g/cc0.0365 lb/in³
Viscosity 1470 cP1470 cP
 200 cP
@Temperature 60.0 °C
200 cP
@Temperature 140 °F
 1000 cP
@Temperature 32.0 °C
1000 cP
@Temperature 89.6 °F
Storage Temperature 15.0 - 60.0 °C59.0 - 140 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.020<= 0.020[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 218 °C424 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.030 %<= 0.030 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<50 Pt-Co
Hydroxyl number26.5-29.5 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez®-ter S1019-54 Polyester Polyol
Dow TONE™ 305 Polyol
Dow TONE™ 301 Polyol
Dow SPECFLEX™ NC 630 Polyol
Covestro Acclaim® 703 Polyether Polyol

PCOVEST0007 / 201790

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.