MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow TONE™ 301 Polyol  (discontinued **)
Categories: Fluid

Material Notes: TONE™ 0301 polyol is a very low equivalent weight tri-functional liquid polyol for use in urethane cast elastomers, coatings and foams.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.084 g/cc1.084 g/cc
Viscosity Measure 230 cSt
@Temperature 55.0 °C
230 cSt
@Temperature 131 °F
Molecular Weight 300 g/mol300 g/mol
Maximum Moisture Content 0.0300.030wt% water
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.25<= 0.25[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 0.000 - 24.0 °C32.0 - 75.2 °F
 
Descriptive Properties
Hydroxyl Number mg KOH/g561.1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100)
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
Eagle Brass 301 Austenitic Stainless Steel, Annealed
Dow TONE™ 305 Polyol
Dow SPECFLEX™ NC 630 Polyol

PDOW1085 / 30289

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.