MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LEXAN™ OQ4005 PC (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: High Viscosity, UV-stabilized PC for ophthalmic lenses.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.14 %0.14 %23°C/sat; ISO 62
Linear Mold Shrinkage, Flow 0.0077 cm/cm0.0077 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0077 cm/cm0.0077 in/inSABIC method
Melt Flow 8.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
8.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi50 mm/min; ASTM D638
Tensile Strength, Yield 64.0 MPa9280 psi50 mm/min; ASTM D638
Elongation at Break 78 %78 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
Tensile Modulus 2.30 GPa334 ksi50 mm/min; ASTM D638
Flexural Yield Strength 96.0 MPa13900 psi1.3 mm/min, 50 mm span; ASTM D790
 97.0 MPa14100 psi2 mm/min; ISO 178
Flexural Modulus 2.31 GPa335 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 9.10 J/cm17.0 ft-lb/inASTM D256
 1.28 J/cm
@Temperature -30.0 °C
2.40 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D4812
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.8
@Frequency 1.10e+9 Hz
2.8
@Frequency 1.10e+9 Hz
SABIC method
Dissipation Factor 0.0063
@Frequency 1.10e+9 Hz
0.0063
@Frequency 1.10e+9 Hz
SABIC method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 61.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
34.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
@Thickness 6.40 mm
264 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 145 °C293 °FRate B/50; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 0.40 %
@Thickness 2.54 mm
0.40 %
@Thickness 0.100 in
ASTM D1003
Transmission, Visible 87 %
@Thickness 2.54 mm
87 %
@Thickness 0.100 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 270 - 290 °C518 - 554 °FInjection Molding
Zone 1 260 - 280 °C500 - 536 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 310 °C536 - 590 °F
Melt Temperature 280 - 310 °C536 - 590 °F
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10528 / 243995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.