MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ OQ4005 PC (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: High Viscosity, UV-stabilized PC for ophthalmic lenses.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.14 %23°C/sat; ISO 62
Linear Mold Shrinkage, Flow 0.0077 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0077 cm/cmSABIC method
Melt Flow 8.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 64.0 MPa50 mm/min; ASTM D638
Elongation at Break 78 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
Tensile Modulus 2300 MPa50 mm/min; ASTM D638
Flexural Yield Strength 96.0 MPa1.3 mm/min, 50 mm span; ASTM D790
 97.0 MPa2 mm/min; ISO 178
Flexural Modulus 2310 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 910 J/mASTM D256
 128 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
 NB
@Temperature -30.0 °C
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.8
@Frequency 1.10e+9 Hz
SABIC method
Dissipation Factor 0.0063
@Frequency 1.10e+9 Hz
SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 61.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 145 °CRate B/50; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 0.40 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 87 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 270 - 290 °CInjection Molding
Zone 1 260 - 280 °C
Zone 2 270 - 290 °C
Zone 3 280 - 310 °C
Melt Temperature 280 - 310 °C
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10528 / 243995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.