MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems CastForm™ PS Plastic for SLS® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: For use with all selective laser sintering (SLS®) systems.

    Applications
  • Create patterns directly rather than through indirect methods
  • Complex investment casting patterns
    • Reactive metals like titanium
    • Low melt-temperature metals such as aluminum, magnesium and zinc
    • Ferrous and non-ferrous metals
  • Economic, low-volume production castings without tooling
  • Smaller parts can be joined to create very large patterns
  • Sacrificial, expendable patterns

    Features
  • Functions like foundry wax and is “foundry friendly”
  • Low residual ash content (< 0.02%)
  • Short burnout cycle
  • Easy-to-process plastic
  • Good plastic powder recycle characteristics

All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.860 g/cc0.860 g/ccASTM D792
Ash <= 0.20 %<= 0.20 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2.84 MPa412 psiASTM D638
Tensile Modulus 1.604 GPa232.6 ksiASTM D638
Izod Impact, Notched <= 0.110 J/cm<= 0.206 ft-lb/inASTM D256
Izod Impact, Unnotched 0.140 J/cm0.262 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems DuraForm® AF Nylon for SLS® Systems
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
3D Systems DuraForm® PA Nylon for SLS® Systems
3D Systems DuraForm® GF Glass Filled Nylon

PAPPR122 / 83501

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.