For use with all selective laser sintering (SLS®) systems.Applications- Create patterns directly rather than through indirect methods
- Complex investment casting patterns
- Reactive metals like titanium
- Low melt-temperature metals such as aluminum, magnesium and zinc
- Ferrous and non-ferrous metals
- Economic, low-volume production castings without tooling
- Smaller parts can be joined to create very large patterns
- Sacrificial, expendable patterns
Features- Functions like foundry wax and is “foundry friendly”
- Low residual ash content (< 0.02%)
- Short burnout cycle
- Easy-to-process plastic
- Good plastic powder recycle characteristics
All information provided by 3D Systems. |
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |