MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

434 Stainless Steel annealed strip
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 400 Series Stainless Steel

Key Words: AFNOR Z 8 CD 17.01 (Fr), UNI X 8 CrMo 17, JIS SUS 434, SS14 2325 (Sweden), UNS S43400, ASTM A651, SAE J405 (51434), DIN 1.4113, B.S. 434 S 19
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8585
Tensile Strength, Ultimate 517 MPa75000 psi
Tensile Strength, Yield 345 MPa
@Strain 0.2 %
50000 psi
@Strain 0.2 %
Elongation at Break 25 %25 %in 50 mm
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000600 ohm-cm
@Temperature 20.0 °C
0.0000600 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 600 - 1100600 - 1100annealed condition at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.4 µm/m-°C
@Temperature 0.000 - 100 °C
5.78 µin/in-°F
@Temperature 32.0 - 212 °F
 11.0 µm/m-°C
@Temperature 0.000 - 315 °C
6.11 µin/in-°F
@Temperature 32.0 - 599 °F
 11.3 µm/m-°C
@Temperature 0.000 - 540 °C
6.28 µin/in-°F
@Temperature 32.0 - 1000 °F
 11.9 µm/m-°C
@Temperature 0.000 - 650 °C
6.61 µin/in-°F
@Temperature 32.0 - 1200 °F
 12.4 µm/m-°C
@Temperature 0.000 - 815 °C
6.89 µin/in-°F
@Temperature 32.0 - 1500 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  26.1 W/m-K
@Temperature 100 °C
181 BTU-in/hr-ft²-°F
@Temperature 212 °F
 26.3 W/m-K
@Temperature 500 °C
183 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1425 - 1510 °C2597 - 2750 °F
Solidus 1425 °C2597 °F
Liquidus 1510 °C2750 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Chromium, Cr 16 %16 %
Iron, Fe 81 %81 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 1.0 %1.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
416 Stainless Steel
430 Stainless Steel annealed at 815°C
434 Stainless Steel annealed sheet
Free-Cutting Brass, UNS C36000
434 Stainless Steel annealed plate

MQ434O / 13167

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.