MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Shandong Dongyue Polymer DF-31B PTFE Pelletized Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Usage: The resin is used to auto press molding and ram extrusion all kinds of rods, pipe etc.

Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.

Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.

Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.

Conformable with Q/DYG 006-2004

Information provided by Shandong Dongyue Polymer Material Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.700 - 0.900 g/cc0.0253 - 0.0325 lb/in³
Particle Size 500 - 700 µm500 - 700 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 20.0 MPa>= 2900 psi
Elongation at Break >= 200 %>= 200 %
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.040 %<= 0.040 %
 
Descriptive Properties
For FabricationAuto press molding and ram extrusion
Powder Flow (g/min)700
Smoothness & CleanlinessGrade 1: Test impurity quantity that equal or less than 1mm doesn't exceed two
 Qualified: Test plate is white and homogeneous, no metal impurities, total impurity quantity <6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shandong Dongyue Polymer DF-21 PTFE Presintered Resin
Shandong Dongyue Polymer DF-31A PTFE Pelletized Resin
Shandong Dongyue Polymer DF-21C PTFE Presintered Resin
Shandong Dongyue Polymer DF-21B PTFE Presintered Resin
Shandong Dongyue Polymer DF-21A PTFE Presintered Resin

PSHADP13 / 103664

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.