MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain CHR® M851 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: CHR® M-Series (1 Mil PET/Rubber adhesive) is manufactured from polyester film with rubber pressure-sensitive adhesive.

Features/Benefits: M851 is designed to use as a flash mask protection tape in metal or composite bonding. The thermosetting rubber adhesive system offers excellent quick-stick properties and flag resistance, yet unwinds easily. The polyester backing resists damage from sharp edges. Polyester backings offer low-cost, effective holding for materials. Operating temperature is -18 to +163 °C, elongation % at break is 100, tensile strength is 44N/cm and dielectric strength is 5,000 volts.

Applications: M851 offers economical methods to hold, insulate and/or protect various materials.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 100 %100 %
Tear Strength 4.38 kN/m25.0 pliInitial Tear Strength
Peel Strength 0.160 kN/m0.913 pliAdhesion to Steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown 6000 V6000 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -17.8 °C0.000 °F
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 910-10X##-P1 0.010" (0.254 mm) Cured Self-fusing Silicone Tape
Aremco Pyro-Tape™ 682-TB2-1 Thermal Barrier Ceramic Tape
Aremco Pyro-Tape™ 682-TB1-2 Thermal Barrier Ceramic Tape
3M Nextel™ BP-18 Woven Tape 312 (5.1 cm)
3M Nextel™ BP-18 Woven Tape 312 (3.8 cm)

PSTGQZ323 / 68837

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.